Many persons working in the construction or engineering industry may find metal as one of the most flexible materials to work with. Considering that it has a large variety of alloys and can be applied to several projects, one can easily see its overall appeal. However, there are certain instances where its durability can become a safety issue. Here are some things you need to know about rust pitting.

First of all, pitting corrosion involves the molecular and physical deconstruction of a metal at a particular area. When left ignored for too long this can result in the formation of miniature holes or cavities which evidently cause the material to become unstable. This results in numerous safety issues brought by corroded projects like bridges, roofs, and even streets.

There are several factors that can attribute to the cause of this issue. Regardless of how stable or durable your material is, the number one factor that causes pitting is the environment where natural processes can break down the components of your metal. Some examples of items easily susceptible to this phenomenon include stainless steel, stainless alloy, and aluminum alloy to name a few.

Another instance that contributes to pitting is not choosing the right kind of component for your project. For instance, low alloy metals are generally more susceptible to cavity formation due to its composition. In fact, most high alloys are generally less likely to rust and can be used in a number of different projects thus making it a more desirable choice.

Another instance that can cause pitting is when the owner does a poor job of applying protecting coating. This element is necessary in keeping your metal firm and stable while also withstanding against various environmental process. When this process is neglected, one can expect a shorter lifespan on their project which can lead to accidents.

With these factors to keep in mind, clients are expected to follow a series of preventive steps before they set off to work their project. One example is selecting the right kind of material that best suits your project. To reduce your chances of developing corrosion later on, consider using options with higher alloy compared to ones with lesser amount.

One such example is the Point Pleasant Bridge or the Silver Bridge. This structure was used to connect Ohio and West Virginia where in nineteen sixty seven, it collapsed and broke down over the river. The incident resulted in at least forty six fatalities where eleven people were injured. After a thorough investigation, it was concluded that stress corrosion was the initial cause.

Last is having a sense of control over certain factors. Indoor projects that involve metal can be kept safe from harm by following certain measures. These include making sure your pH levels, chloride concentrations, and temperatures are at an ideal setting. Otherwise, it could lead to exacerbation of pit formation thus shortening the lifespan of your hard work.

Last but not least is to apply proper industrial coating. Projects that are meant to be placed outside run the risk of incurring environmental damage caused by shifting weather and temperatures. In order to keep them functioning for a long time, make sure to utilize industrial coating to your materials to keep them safe. Additionally, it also helps to check your project every so often to see whether or not they stay stable. Good luck.